Additives and functional resins for coatings and inks
Additives for new energy applications
Additives for semiconductor use
Item |
Specification |
Test Method/Equipment |
Test Standard |
Composite |
Modified styrene maleic anhydride copolymer solution |
--- |
--- |
Appearance |
Yellow transparent liquid |
--- |
--- |
Content |
50% |
Electric hot blast drying oven |
GB/T 1725-2007 |
Solvent |
Water |
--- |
--- |
Density |
1.04-1.06 g/ml |
Pycnometer |
GB/T 6750-2007 |
Viscosity |
1000-5000 mPa.s |
Digital rotary viscometer |
GB/T 15357-2014 |
pH value |
9-13 |
Glass electrode method |
GB/T 9724-2007 |
Refractive index |
1.437-1.441 |
Abbe refractometer |
GB/T 6488-2008 |
Go