Additives and functional resins for coatings and inks
New energy, semiconductor additives
XOANONS®Dispersant
Used for solvent-based system nano-inorganic powder slurry
Product Number
XOANONS®LD 1132B-50
Physical and chemical indexes
Item |
Indexes |
Test method or device |
Detection standard |
|
Composition |
Solutions of styrene-maleic acid copolymers |
--- |
--- |
|
Appearance |
Yellow to orange transparent liquid |
--- |
--- |
|
Solid content |
50±3 % |
Electric Heating Hot Air Oven |
GB/T 1725-2007 |
|
Density |
1.03-1.07 g/ml |
Specific Gravity cup |
GB/T 6750-2007 |
|
Viscosity |
100-500 mPa·s |
Digital rotating viscometer |
GB/T 15357-2014 |
|
pH value |
7.00-10.00 |
Glass electrode method |
GB/T 9724-2007 |
|
Refraction index |
1.451-1.455 |
Abbe refractometer |
GB/T 6488-2008 |
Note: These indexes are representative of typical results and are not to be considered specifications, subject to specific COA.
ApplicationField Dispersing and thixotropy of nano-inorganic powders such as alumina, silicon carbide, silicon nitride, barium titanate, nickel powder, etc. in solvent-based systems
Main features
Usage Firstly, add the dispersant XOANONS®LD 1132B-50 to the solvent, stir well, and then add the powder material according to the formula and disperse it together for grinding.
Suggested Usage Addition amount ( purchase form ) based on 2-10% of powder. (As the optimal addition amount of the dispersant needs to be determined through multiple trials due to different types of powder)
Storage stability Sealed, store in a cool place away from light. Keep for 24 months in the original packaging. Products exceeding the storage period can continue to be used after inspection. The container must be tightly closed immediately after use, before it is completely empty.
Packaging 25 kg (in plastic drums)