Anhui Xoanons Chemical Co.,Ltd.

Anhui Xoanons Chemical Co., Ltd.

PRODUCTS

XOANONS®Additive

Surfactant
Polyacrylate leveling agent
Fluorocarbon modified polyacrylate leveling agent
Fluorine surfactant
Polyether modified silicon leveling agent
Reactive silicon additive with acrylic functional group
Substrate wetting agent
Anti-graffiti additive
Performance enhancer
Dispersant
Defoamer

JIAZHI® Easy-cleaning functional resin

Anti-graffiti and Anti-adhesive Resin for municipal engineering paint
Anti-pollution and rain-resistant resin for protective film of paint
Easy-cleaning resin for industrial paint
Anti-icing resin
Anti-graffiti resin for automotive leather and sofa leather
Anhui Xoanons Chemical Co.,Ltd.

PRODUCTS

Jiazhi®JZ-8600

Model number
JIAZHI®JZ-8600

Specification
Composition: Aqueous silicone modified acrylic dispersion
Appearance: Creamy liquid
Solvent: Water/ Dipropylene Glycol butyl ether
Active content: 41%
PH: 6.5-7.5
Viscosity: 30-2000mPa·s
(Rotating viscometer)(25±0.2)℃
Hydroxyl value: 144±5mg KOH/g
(Theoretical value of solid resin)
Note: This data sheet is intended to give typical results, not
standard.Subject to COA.
Application system
Water-based coating
Properties
Increase slip, hydrophobicity, oil repellency.
Good performance of fouling resistance.
Excellent ability of chemical/solvent resistance.
Good weather-resistance.
Fast drying.

Recommended formula

Part A

material

dosage

function

JIAZHI®JZ-8600

80.00

Base material

DBG

2.00

Diethylene glycol butyl ether

Di-Water

17.00

Deionized water

XOANONS®WE-D547

0.50

Weting agent, XOANONS

Foamex 825

0.20

Defoamer agent, Tego

AMP-95

0.30

PH regulator, Dow

Total

100.00

/

Part B

Aquolin® 161

90.00

Aqueous isocyanate, WANHUA

PMA

10.00

Propylene glycol methyl ether acetate

Total

100.00

/

Note:
·The curing agent is recommended to be used with Wanhua aquolin ® 161, diluted to 90% with PMA, and the matching ratio is 3:1. Add 20-30% deionized water for roller coating and 30-40% deionized water for spraying coating.
·A and B components shall be fully stirred evenly after mixing (machine can be used to disperse if possible). After mixing, under the condition of cover, the storage time is 4-6 hours, so the mixed materials shall be used up as soon as possible.

Dry method
Suggest 80℃, 1-2h
It also has a good effect after self-drying, and the performance can be fully reflected only after curing for more than one week.

Storage stability
Storage: Should store in cool and dry place. Storage temperature should be 5-35 ℃, keep the packaging integrity. Shelf life is 6 months. If over 6 months, it still can be used after pass the performance assessment.

Package
25KG / 180KG